{"version":"1.0","provider_name":"\u5ec8\u9580Carbonsphere\u30c8\u30ec\u30fc\u30c7\u30a3\u30f3\u30b0\u6709\u9650\u516c\u53f8.","provider_url":"https:\/\/www.thefullerene.com\/ja","author_name":"XCT Research Team","author_url":"https:\/\/www.thefullerene.com\/ja\/author\/huangjunkang01foxmail-com\/","title":"C60 XPS: C 1s\u30b9\u30da\u30af\u30c8\u30eb\u3068\u30d5\u30e9\u30fc\u30ec\u30f3\u8868\u9762\u5316\u5b66\u306e\u89e3\u91c8\u65b9\u6cd5","type":"rich","width":600,"height":338,"html":"<blockquote class=\"wp-embedded-content\" data-secret=\"YAhVvS5KiI\"><a href=\"https:\/\/www.thefullerene.com\/ja\/c60-xps-surface-analysis\/\">C60 XPS: C 1s\u30b9\u30da\u30af\u30c8\u30eb\u3068\u30d5\u30e9\u30fc\u30ec\u30f3\u8868\u9762\u5316\u5b66\u306e\u89e3\u91c8\u65b9\u6cd5<\/a><\/blockquote><iframe sandbox=\"allow-scripts\" security=\"restricted\" src=\"https:\/\/www.thefullerene.com\/ja\/c60-xps-surface-analysis\/embed\/#?secret=YAhVvS5KiI\" width=\"600\" height=\"338\" title=\"\u201c\u300cC60 XPS\uff1aC 1s\u30b9\u30da\u30af\u30c8\u30eb\u3068\u30d5\u30e9\u30fc\u30ec\u30f3\u8868\u9762\u5316\u5b66\u306e\u89e3\u91c8\u65b9\u6cd5\u300d \u2014 \u53a6\u9580Carbonsphere\u8cbf\u6613\u6709\u9650\u516c\u53f8.\" data-secret=\"YAhVvS5KiI\" frameborder=\"0\" marginwidth=\"0\" marginheight=\"0\" scrolling=\"no\" class=\"wp-embedded-content\"><\/iframe><script>\n\/*! This file is auto-generated *\/\n!function(d,l){\"use strict\";l.querySelector&&d.addEventListener&&\"undefined\"!=typeof URL&&(d.wp=d.wp||{},d.wp.receiveEmbedMessage||(d.wp.receiveEmbedMessage=function(e){var t=e.data;if((t||t.secret||t.message||t.value)&&!\/[^a-zA-Z0-9]\/.test(t.secret)){for(var s,r,n,a=l.querySelectorAll('iframe[data-secret=\"'+t.secret+'\"]'),o=l.querySelectorAll('blockquote[data-secret=\"'+t.secret+'\"]'),c=new RegExp(\"^https?:$\",\"i\"),i=0;i<o.length;i++)o[i].style.display=\"none\";for(i=0;i<a.length;i++)s=a[i],e.source===s.contentWindow&&(s.removeAttribute(\"style\"),\"height\"===t.message?(1e3<(r=parseInt(t.value,10))?r=1e3:~~r<200&&(r=200),s.height=r):\"link\"===t.message&&(r=new URL(s.getAttribute(\"src\")),n=new URL(t.value),c.test(n.protocol))&&n.host===r.host&&l.activeElement===s&&(d.top.location.href=t.value))}},d.addEventListener(\"message\",d.wp.receiveEmbedMessage,!1),l.addEventListener(\"DOMContentLoaded\",function(){for(var e,t,s=l.querySelectorAll(\"iframe.wp-embedded-content\"),r=0;r<s.length;r++)(t=(e=s[r]).getAttribute(\"data-secret\"))||(t=Math.random().toString(36).substring(2,12),e.src+=\"#?secret=\"+t,e.setAttribute(\"data-secret\",t)),e.contentWindow.postMessage({message:\"ready\",secret:t},\"*\")},!1)))}(window,document);\n\/\/# sourceURL=https:\/\/www.thefullerene.com\/wp-includes\/js\/wp-embed.min.js\n<\/script>","thumbnail_url":"https:\/\/www.thefullerene.com\/wp-content\/uploads\/2026\/07\/ChatGPT-Image-2026\u5e747\u670821\u65e5-16_20_25-1-720x405.png","thumbnail_width":600,"thumbnail_height":338}